Faylka Naxaasta ah ee Profile aadka u hooseeya (VLP-SP/B)
Daawaynta hoose ee micro-roughening waxay si weyn u kordhisaa aagga dusha sare iyada oo aan saamaynaynin qallafsanaanta, taas oo si gaar ah waxtar u leh kordhinta xoogga adhesionka.Iyada oo ku dheggan walxaha sare, ma jiraan wax werwer ah oo qaybuhu ka dhacaan iyo khadadka wasakhaysan.Qiimaha Rzjis ka dib qallafsanaanta waxaa lagu ilaaliyaa 1.0 µm iyo daahfurnaanta filimka ka dib marka la dhejiyo sidoo kale waa wanaagsan yahay.
●Dhumucda: 12um 18um 35um 50um 70um
●Balaadhka caadiga ah: 1290mm, kala duwanaanta ballaca:200-1340mm, waa la jari karaa iyadoo loo eegayo cabbirka cabbirka.
●Baakad sanduuq alwaax ah
●Aqoonsiga: 76 mm, 152 mm
●Dhererka: La habeeyay
●Muunad waa la keeni karaa
Foil-ka la daweeyay waa biibiile naxaas ah oo casaan ah ama midab madow oo qallafsan oo aad u hooseeya.Marka la barbar dhigo foornada naxaasta ah ee elektrolytic-ka caadiga ah, foil-ka VLP-ga waxa uu leeyahay kiristaalo fiican, kuwaas oo u dhigma kuwa tiirar siman leh, oo leh qallafsanaan dusha sare ee 0.55μm, oo leh mudnaanta sida xasilloonida cabbirka wanaagsan iyo qallafsanaanta sare.Alaabtan ayaa lagu dabaqi karaa qalabka xawaaraha sare iyo xawaaraha sare leh, inta badan looxyada wareegyada dabacsan, looxyada wareegyada soo noqnoqda, iyo looxyada wareegyada ultra-fine.
●Muuqaal aad u hooseeya
●Qiimaha ugu sarreeya saamiyada MIT
●Etchability heer sare ah
●2lakab 3lakab FPC ah
●EMI
●Qaab wareeg ah oo fiican
●Taleefanka gacanta ku dallacaadda Wireless
●looxa soo noqnoqda sare
Kala soocidda | Unug | Shuruudaha | Habka Imtixaanka | |||||
Dhumucda magacaaban | Um | 12 | 18 | 35 | 50 | 70 | IPC-4562A | |
Miisaanka Goobta | g/m² | 107±5 | 153± 7 | 285± 10 | 435±15 | 585± 20 | IPC-TM-650 2.2.12.2 | |
daahirnimo | % | ≥99.8 | IPC-TM-650 2.3.15 | |||||
qallafsanaan | Dhinaca dhalaalaya (Ra) | Sam | ≤0.43 | IPC-TM-650 2.3.17 | ||||
Matte side (Rz) | um | ≤3.0 | ≤3.0 | ≤3.0 | ≤3.0 | ≤3.0 | ||
Xoogga Jilicsan | RT(23°C) | Mpa | ≥300 | IPC-TM-650 2.4.18 | ||||
HT(180°C) | ≥180 | |||||||
Dheeraynta | RT(23°C) | % | ≥5 | ≥6 | ≥8 | ≥10 | ≥10 | IPC-TM-650 2.4.18 |
HT(180°C | ≥6 | ≥6 | ≥6 | ≥6 | ≥6 | |||
Xoogga diirka (FR-4) | N/mm | ≥0.8 | ≥0.8 | ≥1.0 | ≥1.2 | ≥1.4 | IPC-TM-650 2.4.8 | |
lbs/in | ≥4.6 | ≥4.6 | ≥5.7 | ≥6.8 | ≥8.0 | |||
Godadka & Porosity | Tirooyinka | No | IPC-TM-650 2.1.2 | |||||
Anti-oksidization | RT(23°C) | Days | 180 | |||||
HT(200°C) | Daqiiqado | 30 | / |